Glow in the dark Glass process
For Glow in the dark Glass process, We suggest our?High-temperature resistance glow in the dark pigment, YG-405-RH has?an excellent high-temperature?performance, you can mix the glow in the dark pigment with melted glass. To make sure the glow in the dark glass has a perfect glow effect you should pay?attention to following items.
1. Generally, the glow in the dark pigment can?withstand 1250 ℃ for less than 30 minutes. Before you make the glow in the dark Glass product, we suggest you test the pigment first. You can also?Consult us and tell us the details about you glow in the dark glass process, we can also do the OEM for you.
2. The glass?Raw materials should be transparent. More transparent the glass is,?the glow effect will be better.
?
?
Product |
?
Glow Color |
The Average Particle Size D50 (mesh) |
Afterglow Brightness (mcd/m2) | ?
?TDS Download |
|
10min | 60min | ||||
YG-405-RH | ?Yellow-Green | 20 | 1268 | 166 | ?DOWNLOAD |
We have various color glow in the dark pigment, such as yellow, red, white, lemon green, green, pink red and etc. you can find the details of color glow in the dark pigment below.